Metallic Yarn
PROPERTIES OF METALLIC YARN
Metallic yarn have the following chemical characteristics:
| ironing | 15 sec at 110°C |
| dry heat | 60 sec at 180°C |
| alkali, solution of 1st process | 30 min at pH 4.7 |
| hot water | 30min at 90°C |
| hand washing | 0.5% soap, 0.2% sodium carbondate anhydride, 30 min at 60°C |
| rubbing | 200g, 100 time |
| dry cleaning | trichloroethylene, perchloroethylene or petroleum benzene; 30min at 25°C |
| steaming | 40min at 100°C |
| boiling water | 30-60 min |
| acid | 2% oxalic adic or 2% acetic acid for 10min at 60°C |
| scouring for supports / twists of metallic yarn | Soda Ash, 1 g/l for 30min at 60°C |
| customs tariff number | 5605.00.100 |